EN353 Grade Introduction:
We are EN353 Alloy Steel Round Bar manufacturers and we are manufacturing from prime quality billets and blooms. The range of EN353 Round Bars which we manufacture for our customers are of high quality and these round bars are used for making machinery and Auto components. These products have been made keeping in mind the quality parameters that have been set by the industry in the market. EN353 Round Bars are always supplied with the test certificates and can be supplied in bulk quantity as well as retail quantity as per customer’s requirements. EN353 alloy Steel round bars are supplied by us to various industries.
EN353 Alloy steel is a very high strength steel alloy that is hardened and tempered before supplying and has nickel, chromium, molybdenum making its high tensile steel strength, with good ductility and wear resistance. With relatively good impact properties at low temperatures, EN353 is also suitable for a variety of elevated temperature applications. EN353 round bars have good internal strength and high external strength, which makes them highly wear-resistant. EN353 steel round bars offer a good combination of ductility, strength, and wear resistance. EN353 is a very high-strength alloy engineering steel.
EN353 Grade Application:
Acceptable for many automobile applications such as heavy-duty gear, shaft, pinion, camshafts, gudgeon pins.
EN353 Equivalent grades:
BRITISH BS 970:1991 815M17
BRITISH BS 970:1955 EN353
GERMAN DIN 20NiCrMo5
FRENCH AFNOR 20NCD5
SWEDISH SS 2523
EUROPEAN STEEL NAME 17NiCrMoS6-4
EUROPEAN STANDARD EN10277-4
Addition to other grades:
MS, EN1A, EN3B, EN8, EN8D, EN9, EN24, EN31, EN32B, EN36C, EN41B, EN43B, EN47, EN353, IS2062, 42Crmo4, HCHCR, D2, D3, H-11, H-13, CW-1, OHNS M2, M35, M42, DIN-1.2714, P20, P20+S, P20+Ni, SCM420, ASTMSA-36, ASTM SA-105 , SAE1018, SAE1010, SAE4140, SAE8620, 16MNCR5, 20MNCR5, C20, C45, C50, C60, CK45, 20C8, 40C8, 45C8, 55C8, C55MN75, SAE52100, S40C, S355J2G3.
Our Supply Range:
Price List:
EN353 Chemical composition:
The following table shows the chemical composition of EN353 steel:
Element |
C |
Si |
Mn |
S |
P |
Ch |
Mo |
Ni |
Content (%) |
0.10-0.20 |
0.10-0.35 |
0.50-1.00 |
0.040 Max |
0.040 Max |
0.75-1.25 |
0.08-0.15 |
1.00-1.50 |
EN353 Mechanical Properties:
Mechanical Properties |
|
Hardening |
840-870 |
Quenching |
oil |
Tempering |
150-200 |
Brinell Rockwell Hardness |
150-200 |
EN353 Other Details of Property
Annealed |
R |
S |
T |
U |
V |
W |
Y |
|
Ruling Section (mm) |
150 |
150 |
100 |
65 |
65 |
30 |
30 |
25 |
Tensile Strength (MPa) |
680/720 |
690/850 |
770/930 |
850/ 1000 |
930/ 1080 |
1000/1160 |
1080/1240 |
1280 |
Yield Stress (MPa) |
440/480 |
480 |
570 |
665 |
740 |
835 |
895 |
1050 |
Elongation (% Min) |
22 |
15 |
15 |
13 |
12 |
12 |
10 |
10 |
ISO V Impact (Joule) |
30 |
30 |
30 |
30 |
25 |
25 |
22 |
7 |
Hardness (Brinell) |
190/210 |
201/255 |
223/277 |
248/ 302 |
269/ 321 |
293/ 341 |
311/ 375 |
363/415 |
Proof Stress (0.2%) if required (MPa, Min) |
495 |
550 |
630 |
710 |
770 |
850 |
985 |
EN353 Hardness:
HB – 270
EN353 Heat treatment:
The hardening treatment for most steels consists of heating the steel to a set temperature and then cooling it rapidly by plunging it into oil, water. EN8 and EN353 steel is an easily available and cheap material that is acceptable for heavy-duty applications.
EN353 Hardening:
Hardening °C 780-820.
EN353 Tempering:
EN353 is re-heated to 780C – 820°C, holding until the temperature is uniform throughout the section, and then quenched in oil, Tempering must be done immediately while the component EN353 is still handed warm. Heat to 150C – 200°c, soak it for 1 – 2 hours / 25mm of a section, and then cooled in still air. Hardness after Tempering: 62-64 HRC.
EN353 Physical Properties:
Thermal Conductivity at °C |
20 |
350 |
700 |
W/(m*K) |
11.3 |
13.3 |
14.5 |
EN353 Thermal Properties:
Thermal Conductivity at °C |
20 |
350 |
700 |
W/(m*K) |
11.3 |
13.3 |
14.5 |
EN353 Forging Properties:
EN353 steel round bars offer a good combination of ductility, strength, and wear resistance. EN353 is a very high-strength alloy engineering steel.
EN353 Stress Relieving:
150-200, cooled in the furnace.
1st pre-heating °C: Up to approx. 400 in an air-circulating furnace
2nd and 3rd: 780 and 805°C.
EN353 Normalizing:
860 – 890°C in air.
EN353 Annealing:
630-670°C
EN353 Density:
DENSITY (G/CM 3) |
8.08 |
DENSITY (LB/IN 3) |
0.292 |
EN353 Machinability:
75
EN353 Welding:
Pre/post heat precaution required.
Supply Cities:
Ahmedabad, Amaravathi, Ambattur, Bangalore, Belgaum, Chennai, Chittoor, Coimbatore, Dindigul, Mysore, Nellore, Hyderabad, Kochi, Mangalore, Tirupur, Tuticorin, Madurai, Andhra Pradesh, Karnataka, Puducherry, Kerala, Tamil Nadu, Telangana, Salem, Thanjavur, Trichy, Erode, Vellore, Ranipet, Sivakasi, Karur, Hosur, Nagercoil, Kanchipuram, Karaikudi, Neyveli, Cuddalore, Kumbakonam, Thiruvannamalai, Pollachi, Rajapalayam, Gudiyatham, Pudukottai, Vaniyambadi, Ambur, Nagapattinam, Trivandrum, Vijayawada, Guntur, Thirupathi, Nazarathpet, Kakinada, Kurnool, Kadapa, Nizamabad, Mahabubnagar, Karimnagar.
People also search as:
EN353 Steel Round Bar, EN353 Steel Round Bar Manufacturers, EN353 Steel Suppliers, EN353 Stockist, EN353 Steel Dealers, EN353 Steel Distributors, EN353 Wholesalers, EN353 Steel Traders, EN353 Steel Square Distributors, EN353 Steel Flat Bar, EN353 Steel Companies Near me.
EN353, EN353 Steel, EN353 Chemical composition, EN353 Mechanical properties, EN353 Equivalent Grades, EN353 Steel plate, EN353 Steel sheet, EN353 Manufacturers, EN353 Suppliers, EN353 Dealers, EN353 Stockist, EN353 Distributors, EN353 Wholesalers, EN353 Traders.
Metal Weight Calculator:
Shape:
Quantity:
Diameter:
Length:
Results
Calulated Weight: 0 Kgs / 0 Lbs